Surface State of tungsten bar:
Any oxidation, contamination, and
severe excessive fusion, bubbling, delamination, or crack is not
allowed for product W1. Camber should be no more than 10mm. Any
excessive fusion, bubble, delamination, crack, surface bulky
crystallization or severe oxidation &contamination are not allowed
for products W2 and W3. The length of the spalls should not be more
than 8mm, width no more than 3mm, depth no more than 1mm; The diameter
of mechanical pitting should not be more than 1mm, depth no more than
0.5mm; Camber should be no more than 4mm.
Any oxidation or contamination is not allowed for product w4.
The cartridge of the vertical sintering part should be cut off, and the section is not allowed to be loose or intermingled.
Any oxidation or contamination is not allowed for product w4.
The cartridge of the vertical sintering part should be cut off, and the section is not allowed to be loose or intermingled.